Customization: | Available |
---|---|
Certification: | ISO, RoHS |
Technique: | Winding Filament Roving |
Still deciding? Get samples of US$ 1/Piece
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Model Number | Linear Density(Tex) | Moisture Content% | Size Content% | Breaking Strength(N/tex) |
EDR300-T908 | 300±5% | ≤0.20 | 0.55±0.20 | ≥0.35 |
EDR600-T908 | 600±5% | ≤0.20 | 0.55±0.20 | ≥0.35 |
EDR900-T908 | 900±5% | ≤0.20 | 0.55±0.20 | ≥0.35 |
EDR1200-T908 | 1200±5% | ≤0.20 | 0.55±0.20 | ≥0.35 |
EDR1500-T908 | 1500±5% | ≤0.20 | 0.55±0.20 | ≥0.35 |
EDR2400-T908 | 2400±5% | ≤0.20 | 0.55±0.20 | ≥0.35 |
EDR4800-T908 | 4800±5% | ≤0.20 | 0.55±0.20 | ≥0.35 |
Item | Testing Method and Standard | |
Testing Method | Standard | |
Oil content | ISO1887 | 0.55±0.15 |
Roving Linear weight (tex) | ISO1889 | 2400±5 % |
Moisture content | ISO3344 | ≤0.10 |
Breaking Tensile Strength | ISO3375 | ≥0.35 |